The Professional Induction Brazing Stainless Steel Tubing Joints Technology
The goal of this induction brazing application test is for Induction Brazing Stainless Steel Tubing Joints evenly for increased repeatability.

Process:
The two stainless tubes where joined together and an alloy ring was placed around the joint. Black flux was then applied to the joint for a better induction brazing process. The work piece was placed inside the helical coil for 15 seconds where 8 kW of induction heating power was applied. The work piece reached 1472°F (800°C) and was successfully brazed. The HLQ induction heating equipment recommend for this application is the DW-UHF-10KW induction brazing heater along with a 10 kW power supply.