Brazing Carbide to Steel Part With Induction Heating
![](https://dw-inductionheater.com/wp-content/uploads/2021/02/Brazing-carbide-with-induction-heating-1024x505.png)
![](https://dw-inductionheater.com/wp-content/uploads/2021/02/induction-brazing-carbide-to-steel-process-1024x517.png)
![](https://dw-inductionheater.com/wp-content/uploads/2021/02/induction-brazing-carbide-to-steel-1024x647.png)
Induction Brazing Process:
- To demonstrate elimination of “hand feeding” the alloy, we formed the alloy into a ring to tightly fit over the center post tube. This method provides a uniform amount for each cycle, resulting in uniform joints and wetting.
- The custom made coil was then placed over the steel piece, where is was set for 14 seconds to heat the alloy.
- The alloy was heated at approximately 1500°F (815)°C
- The whole piece is left alone and cooled with ambient air